2K Water-borne Polyurethane sand streak coating


Two component self-drying product with excellent weather resistance, sand streak effect can be customized as request, high hardness, recommended for mechanical equipment with high decorative and protective requirements, and can also be used as powder coating for touch up.

Categorize: Water-borne Industrial Decorative Coating


Product Details


Features & Application

Two component self-drying product with excellent weather resistance, sand streak effect can be customized as request, high hardness, recommended for mechanical equipment with high decorative and protective requirements, and can also be used as powder coating for touch up.
 

Technical Data

Item

Index

Item

Index

Drying Time

Surface Drying Time:≤2h

Hardness

3H

Fully Drying Time: ≤16h

Weather Resistance >500h
Water Resistance >240h

Adhesion/Grade

Grade one

 

Product packages and construction parameters

The previous coat can be matching used with water-based epoxy primer, and other matching materials can be customized as request.

It can be used as powder coating for touch up.

Matching diluent: Distilled water or clean tap water

Operation Way

Dilution Ratio

Working Viscosity

Remark

Air Spraying

6-10%

Cai-4 15-20s

The viscosity of the coating will decrease with the increase of ambient temperature, so the specific working viscosity should be slightly adjusted according to the actual environmental conditions

Pressure Air Spraying

4-8%

Cai-4 25-40s

High Pressure Airless
spraying

3-6%

Cai-4 30-60s



Precautions

The drying effect of water-based coating products is greatly affected by different environmental factors. During application, a comprehensive judgment should be made based on the temperature, humidity, wind speed, and drying conditions of the environment, to achieve the best appearance and performance of the paint film.

The self- recoating interval must be at least 1 hour after the surface dries, and the actual time depends on the impact of different environmental humidity and temperature on product drying; General between 2 hours and 6 hours; It is best to reapply the topcoat with an interval of more than 24 hours.

The operation temperature is between 10℃ and 30℃, and the operation humidity is no more than 75%. It must be thoroughly stirred and evenly mixed before use, and frequent stirring is required during coating, to prevent sedimentation.  

 

Keyword:

2K Water-borne Polyurethane sand streak coating

Recommended Products

Enquire Now

If you are interested in our products, please leave your e-mail, we will contact you as soon as possible, thank you!

Submit Message